Synthesis of Chitosan/Zinc Oxide Nanoparticles Stabilized by Chitosan via Microwave Heating

Nowadays, zinc oxide (ZnO) has attracted attention in research and development because of its remarkable antibacterial properties. Chitosan/ZnO nanoparticles were successfully synthesized via microwave heating. The objectives of this work were to investigate the effect of stabilizer, power heating a...

Full description

Saved in:
Bibliographic Details
Main Authors: Ahmad Yusof, Nurul Amira (Author), Mat Zain, Norashikin (Author), Pauzi, Norlin (Author)
Other Authors: Ministry of Education, Malaysia, and Universiti Malaysia Pahang for financial support (RDU 150333) (Contributor)
Format: EJournal Article
Published: Department of Chemical Engineering - Diponegoro University, 2019-08-01.
Subjects:
Online Access:Get Fulltext
Get Fulltext
Get Fulltext
Get Fulltext
Get Fulltext
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Nowadays, zinc oxide (ZnO) has attracted attention in research and development because of its remarkable antibacterial properties. Chitosan/ZnO nanoparticles were successfully synthesized via microwave heating. The objectives of this work were to investigate the effect of stabilizer, power heating and time heating on size of chitosan/ZnO nanoparticles and to determine antibacterial activity against pathogenic bacteria, where chitosan was used as a stabilizing agent. Chitosan/ZnO nanoparticles were analyzed  by Fourier Transform Infra Red (FTIR), X-ray Diffraction (XRD), Field Emission Scanning Electron Microscopy (FESEM), and Zetasizer instrument. The power heating and time heating were varied from 400 to 800 Watt and 4 to 8 minutes, respectively. The presence of chitosan has role on preventing the nanoparticles from agglomeration by producing a milky solution of chitosan/ZnO nanoparticles without any suspensions. The increase of power  and time heating improved the size of nanoparticles. The peak in FTIR spectrum at around 427 cm-1 was confirmed the existence of the ZnO phase. XRD patterns showed that the chitosan/ZnO nanoparticles materials were pure phase with average crystalline size is 130 nm. FESEM revealed that chitosan/ZnO nanoparticles were uniformly distributed with the mean value of size is 70 nm and spherical shaped. Further impact of power and time heating on the size of the chitosan/ZnO nanoparticles can be shown by a nanoparticles size distribution with the average of 30 to 90 nm. The results showed that chitosan/ZnO nanoparticles have displayed an antibacterial inhibition zone against Gram-positive S. aureus and Gram-negative E. coli which 16.0 and 13.3 mm, respectively. Chitosan/ZnO nanoparticles were synthesized in this work presented have potential application to prevent bacterial infections. 